In this research AA6060 alloy was used and was extruded at 25m/min, 30m/min, 35m/min, 40m/min and45m/min for a particular profile. The highest exittemperature increased from 542°C to 567°C when theextrusion speed was increased from 25m/min to 45m/min.Three types of die pick-up were identified. They werenamed as normal pick-up, die line pick-up and lumppick-up. Normal pick-up occurred regardless of theextrusion speed and exit temperature; however theamount of normal pick-up did not increase when theextrusion speed was increased. Die line pick-up occurred when the extrusion speed was 45m/min andappeared only on the die lines. Lump pick-up is notsignificant since it was very rare.AA6060 (0.4%Mg and 0.5%Si) alloy has about 0.27% excess silicon and therefore at 555°C, Mg2Siparticles react with aluminium and excess silicon toform liquid. However normal pick-up and die linepick-up still occurred at temperatures lower andhigher than 555°C and therefore it confirms thateutectic reactions do not influence formation of pickup.Therefore die pick-up is most likely to be caused due to a mechanical process ratherthan a metallurgical process.
"synopsis" may belong to another edition of this title.
Robbie Peris was brought up in Sri Lanka and migrated to New Zealand in 2002. He obtained his BE(Hons) and ME(Hons) fromAUT University Auckland New Zealand. He did his Masters Thesiswith Fletcher Aluminium. Currently Robbie Peris is working as aResearch Officer at AUT University and is part of the metalforming group.
"About this title" may belong to another edition of this title.
Seller: GreatBookPrices, Columbia, MD, U.S.A.
Condition: New. Seller Inventory # 5848126-n
Seller: BargainBookStores, Grand Rapids, MI, U.S.A.
Paperback or Softback. Condition: New. Effects of Extrusion Process Conditions on "Die Pick-Up". Book. Seller Inventory # BBS-9783836484312
Seller: PBShop.store US, Wood Dale, IL, U.S.A.
PAP. Condition: New. New Book. Shipped from UK. THIS BOOK IS PRINTED ON DEMAND. Established seller since 2000. Seller Inventory # L0-9783836484312
Seller: Chiron Media, Wallingford, United Kingdom
PF. Condition: New. This item is printed on demand. Brand new book, sourced directly from publisher. Dispatch time is 6-7 days from our warehouse. Book will be sent in robust, secure packaging to ensure it reaches you securely. Seller Inventory # 6666-IUK-9783836484312
Quantity: 20 available
Seller: GreatBookPrices, Columbia, MD, U.S.A.
Condition: As New. Unread book in perfect condition. Seller Inventory # 5848126
Seller: PBShop.store UK, Fairford, GLOS, United Kingdom
PAP. Condition: New. New Book. Delivered from our UK warehouse in 4 to 14 business days. THIS BOOK IS PRINTED ON DEMAND. Established seller since 2000. Seller Inventory # L0-9783836484312
Quantity: Over 20 available
Seller: California Books, Miami, FL, U.S.A.
Condition: New. Seller Inventory # I-9783836484312
Seller: GreatBookPricesUK, Woodford Green, United Kingdom
Condition: New. Seller Inventory # 5848126-n
Quantity: Over 20 available
Seller: GreatBookPricesUK, Woodford Green, United Kingdom
Condition: As New. Unread book in perfect condition. Seller Inventory # 5848126
Quantity: Over 20 available
Seller: AHA-BUCH GmbH, Einbeck, Germany
Taschenbuch. Condition: Neu. nach der Bestellung gedruckt Neuware - Printed after ordering - In this research AA6060 alloy was used and was extruded at 25m/min, 30m/min, 35m/min, 40m/min and45m/min for a particular profile. The highest exittemperature increased from 542°C to 567°C when theextrusion speed was increased from 25m/min to 45m/min.Three types of die pick-up were identified. They werenamed as normal pick-up, die line pick-up and lumppick-up. Normal pick-up occurred regardless of theextrusion speed and exit temperature; however theamount of normal pick-up did not increase when theextrusion speed was increased. Die line pick-up occurred when the extrusion speed was 45m/min andappeared only on the die lines. Lump pick-up is notsignificant since it was very rare.AA6060 (0.4%Mg and 0.5%Si) alloy has about 0.27% excess silicon and therefore at 555°C, Mg2Siparticles react with aluminium and excess silicon toform liquid. However normal pick-up and die linepick-up still occurred at temperatures lower andhigher than 555°C and therefore it confirms thateutectic reactions do not influence formation of pickup.Therefore die pick-up is most likely to be caused due to a mechanical process ratherthan a metallurgical process. Seller Inventory # 9783836484312
Quantity: 2 available