Two different types of alloys, namely alloy- 1 and Alloy-2, have been designed and produced using a melting casting route. Homogenized alloys are further cold rolled to 55- 65% thickness reduction. The rolled material in the case of Alloy-2 is annealed at 490℃ for 4 hours and then subsequently aged for various intervals of times, whereas Alloy 1 is annealed at 5400C for 4 hours. The annealing temperatures are selected based on DSC analysis. Detailed microstructural and precipitations characterizations have been carried out for cast, rolled, and aged samples by Optical Microscopy, SEM, XRD, and EBSD analysis. The precipitates of Mg2Si and Si3Mg2 are observed in both Alloy-1 and Alloy-2, whereas TiB2 is observed in only Alloy-2 due to the presence of Ti and B as a grain refiners. This type of precipitates is observed at peak aged conditions. The mechanical properties like bulk hardness, nano-hardness, and room temperature tensile properties have been studied for both alloys. In case alloy 2, due to the grain refinement effect, the average grain size of the cast sample is reduced from (55.283±1.91) µm to (42.886±1.20) µm.
"synopsis" may belong to another edition of this title.
Seller: Books Puddle, New York, NY, U.S.A.
Condition: New. Seller Inventory # 26397337885
Quantity: 4 available
Seller: Majestic Books, Hounslow, United Kingdom
Condition: New. Print on Demand. Seller Inventory # 400120514
Quantity: 4 available
Seller: Biblios, Frankfurt am main, HESSE, Germany
Condition: New. PRINT ON DEMAND. Seller Inventory # 18397337879
Quantity: 4 available
Seller: BuchWeltWeit Ludwig Meier e.K., Bergisch Gladbach, Germany
Taschenbuch. Condition: Neu. This item is printed on demand - it takes 3-4 days longer - Neuware -Two different types of alloys, namely alloy- 1 and Alloy-2, have been designed and produced using a melting casting route. Homogenized alloys are further cold rolled to 55- 65% thickness reduction. The rolled material in the case of Alloy-2 is annealed at 490 for 4 hours and then subsequently aged for various intervals of times, whereas Alloy 1 is annealed at 5400C for 4 hours. The annealing temperatures are selected based on DSC analysis. Detailed microstructural and precipitations characterizations have been carried out for cast, rolled, and aged samples by Optical Microscopy, SEM, XRD, and EBSD analysis. The precipitates of Mg2Si and Si3Mg2 are observed in both Alloy-1 and Alloy-2, whereas TiB2 is observed in only Alloy-2 due to the presence of Ti and B as a grain refiners. This type of precipitates is observed at peak aged conditions. The mechanical properties like bulk hardness, nano-hardness, and room temperature tensile properties have been studied for both alloys. In case alloy 2, due to the grain refinement effect, the average grain size of the cast sample is reduced from (55.283±1.91) µm to (42.886±1.20) µm. 52 pp. Englisch. Seller Inventory # 9786205499849
Quantity: 2 available
Seller: moluna, Greven, Germany
Condition: New. Dieser Artikel ist ein Print on Demand Artikel und wird nach Ihrer Bestellung fuer Sie gedruckt. Autor/Autorin: Singha PrasenjitM-tech IIT Kharagpur, research scholar IIT Madras.Two different types of alloys, namely alloy- 1 and Alloy-2, have been designed and produced using a melting casting route. Homogenized alloys are further cold roll. Seller Inventory # 731805322
Quantity: Over 20 available
Seller: buchversandmimpf2000, Emtmannsberg, BAYE, Germany
Taschenbuch. Condition: Neu. Neuware -Two different types of alloys, namely alloy- 1 and Alloy-2, have been designed and produced using a melting casting route. Homogenized alloys are further cold rolled to 55- 65% thickness reduction. The rolled material in the case of Alloy-2 is annealed at 490¿ for 4 hours and then subsequently aged for various intervals of times, whereas Alloy 1 is annealed at 5400C for 4 hours. The annealing temperatures are selected based on DSC analysis. Detailed microstructural and precipitations characterizations have been carried out for cast, rolled, and aged samples by Optical Microscopy, SEM, XRD, and EBSD analysis. The precipitates of Mg2Si and Si3Mg2 are observed in both Alloy-1 and Alloy-2, whereas TiB2 is observed in only Alloy-2 due to the presence of Ti and B as a grain refiners. This type of precipitates is observed at peak aged conditions. The mechanical properties like bulk hardness, nano-hardness, and room temperature tensile properties have been studied for both alloys. In case alloy 2, due to the grain refinement effect, the average grain size of the cast sample is reduced from (55.283±1.91) µm to (42.886±1.20) µm.Books on Demand GmbH, Überseering 33, 22297 Hamburg 52 pp. Englisch. Seller Inventory # 9786205499849
Quantity: 2 available
Seller: AHA-BUCH GmbH, Einbeck, Germany
Taschenbuch. Condition: Neu. nach der Bestellung gedruckt Neuware - Printed after ordering - Two different types of alloys, namely alloy- 1 and Alloy-2, have been designed and produced using a melting casting route. Homogenized alloys are further cold rolled to 55- 65% thickness reduction. The rolled material in the case of Alloy-2 is annealed at 490 for 4 hours and then subsequently aged for various intervals of times, whereas Alloy 1 is annealed at 5400C for 4 hours. The annealing temperatures are selected based on DSC analysis. Detailed microstructural and precipitations characterizations have been carried out for cast, rolled, and aged samples by Optical Microscopy, SEM, XRD, and EBSD analysis. The precipitates of Mg2Si and Si3Mg2 are observed in both Alloy-1 and Alloy-2, whereas TiB2 is observed in only Alloy-2 due to the presence of Ti and B as a grain refiners. This type of precipitates is observed at peak aged conditions. The mechanical properties like bulk hardness, nano-hardness, and room temperature tensile properties have been studied for both alloys. In case alloy 2, due to the grain refinement effect, the average grain size of the cast sample is reduced from (55.283±1.91) µm to (42.886±1.20) µm. Seller Inventory # 9786205499849
Quantity: 1 available